Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 145.2 g/mol | 145.2 g/mol | |
BASF BAPMA N,N-Bis-(3-aminopropyl)methylamine Formula: C7H18N3CAS: 105-83-9Description: N,N-Bis-(3-aminopropyl)methylamine is a colorless to yellow liquid, with an amine-like odor. It is miscible with water in all proportion.Synonyms: BAPMA, M.. |