Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 144.3 g/mol | 144.3 g/mol | |
BASF Octamethylenediamine Formula: C8H20N20CAS: 373-44-4Description: Octamethylenediamine is a colorless solidified mass with an amine-like odor. It is miscible with water.Synonyms: 1,8-DiamineoctaneApplications: It is used.. |