Polymer Property : Molecular Weight = 141.1 g/mol Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Molecular Weight 141.1 g/mol
141.1 g/mol
Dow Corning Z-1227 METHYLVINYLDICHLOROSILANE
Information provided by Dow Corning