Molecular Weight 133000 g/mol
133000 g/mol
distribution: 4.5 Mw/Mn; GPC
Borealis FG5190 Linear Low Density Polyethylene
FG5190 is a Butene Linear Low Density Polyethylene for Film Extrusion. Includes Antioxidant. The grade is developed for medium and heavy duty bags, bags and bin liners, dual stretch films, and film..