Physical Properties Metric English Comments
Molecular Weight 128.9 - 146.9 g/mol
128.9 - 146.9 g/mol
Solvay Chemicals CASO® Powder
CASO® Calcium Chloride technical grade can be used in various applications in industrial, public and private sectors.REACH Registration Number: 01-2119494219-28/ CAS number: 10043-52-4 / EINECS -..