Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 126.2 g/mol | 126.2 g/mol | |
BASF Cyclohexyl Vinyl Ether Formula: C8H14O>CAS: 2182-55-0Description: Cyclohexyl vinyl ether is a colorless to yellow liquid, with a sweetish odor. It is soluble in water and with many organic solvent.Synonyms: CHVE, CVE, (Vi.. |