Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 1200 g/mol | 1200 g/mol | Mn; ETM 300-83 |
ExxonMobil ESCOREZ™ 1310 LC Petroleum Hydrocarbon Resin This product is a light colored, premium aliphatic hydrocarbon resin with narrow molecular weight distribution. It is designed to tackify a variety of adhesive polymers including EVA, metallocene .. |
|||
Molecular Weight | 1200 g/mol | 1200 g/mol | Mn; ETM E-83 |
ExxonMobil ESCOREZ™ 1401 (Europe) Petroleum Hydrocarbon Resin ESCOREZ™ 1401 is a modified aliphatic hydrocarbon resin with a narrow molecular weight distribution and a high softening point. It is a tackifying resin designed to provide high temperature perform.. |