Physical Properties Metric English Comments
Molecular Weight 118.2 g/mol
118.2 g/mol
LyondellBasell PNP Propylene glycol normal propyl ether
Information provided by Lyondell.
Molecular Weight 118.2 g/mol
118.2 g/mol
BASF HDO® 1,6-Hexanediol Flakes
Formula: C6H14O2CAS: 629-11-8Description: 1,6-Hexanediol (HDO) flakes are a colorless, odorless solids or molten masses. It is miscible in water in all proportions and soluble in ethanol.Synonyms: ..
Molecular Weight 118.2 g/mol
118.2 g/mol
BASF HDO® 1,6-Hexanediol Molten
Formula: C6H14O2CAS: 629-11-8Description: 1,6-Hexanediol Molten (HDO) is a colorless, odorless molten mass or solid. It is miscible in water in all proportions and soluble in ethanol.Synonyms: Hexa..