Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 1178 g/mol | 1178 g/mol | |
Suqian Unitechem Antioxidant 1010 Chemical Name: Tetrakis [methylene-3-(3,5-di-tert-butyl-4-hydroxyphenyl-propionate)]methaneCAS NO.: 6683-19-8Molecular Formula: C73H108O12Properties: The product takes on the appearance of white pow.. |