Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 104.15 g/mol | 104.15 g/mol | |
LG Chemical NPG Flake Neopentyl Glycol NPG is a diol with two hydroxyl groups located in the 1,3-position on the primary carbon atom. Additionally, it has two methyl groups instead of the usual two hydrogen atoms on the a-carbon atom. It.. |