Physical Properties Metric English Comments
Molecular Weight 1020 g/mol
1020 g/mol
average
Solvay Specialty Polymers Galden® D05 PFPE Fluid
Galden® D grades are specifically recommended for electronic reliability testing, including thermal shock and hermetic seal testing.Galden® PFPE is a line of high-performance, inert, fluorinat..
Molecular Weight 1020 g/mol
1020 g/mol
average
Solvay Specialty Polymers Galden® HT230 PFPE Heat Transfer Fluid
Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service..
Molecular Weight 1020 g/mol
1020 g/mol
average
Solvay Specialty Polymers Galden® LS230 PFPE VPS Fluid
Galden® LS and HS grades are specifically recommended for vapor phase soldering.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of servic..