Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 102.1 g/mol | 102.1 g/mol | |
LyondellBasell Propylene Carbonate Information provided by Lyondell. |
|||
Molecular Weight | 102.1 g/mol | 102.1 g/mol | |
BASF Propylencarbonate S Formula: C4H6O3CAS: 108-32-7Description: Propylencarbonate is a colorless to yellowish liquid, with a fruity odor. It is soluble in water and with many organic solvents.Synonyms: PC, Propylene carb.. |