Polymer Property : Molecular Weight = 100000 g/mol Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Molecular Weight 100000 g/mol
100000 g/mol
ASTM D3536
SK Chemicals SKYTHANE® U0251M Ink Binder
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Molecular Weight 100000 g/mol
100000 g/mol
ASTM D3536
SK Chemicals SKYTHANE® UB601 Ink Binder
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. UB series are used for adhesives and coating applications such as binder for magnetic ta..
Molecular Weight 100000 g/mol
100000 g/mol
Westlake Epolene® C-17 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer
Product Description: Epolene C-17 is a branched low density polyethylene with a relatively high melt point and viscosity compared to other Epolene C-type Polymers. It is useful to modify paraffin wa..
Molecular Weight 100000 g/mol
100000 g/mol
Westlake Epolene® C-17P Coating Grade - Branched Medium Molecular Weight Polyethylene Polymer
Description: Epolene C-17P is a branched low density polyethylene powder with a relatively high melt point and viscosity compared to other Epolene C-type Polymers. It is useful to modify paraffin wa..