Physical Properties Metric English Comments
Molecular Weight 1.10e+6 g/mol
1.10e+6 g/mol
Zeon Chemicals Quintone® D100 Aliphatic Hydrocarbon Resin
C5/C9 type (piperylene and dicyclopentadiene precursor). Has improved compatibility with SBR and EVA; suitable for adhesive tapes and hot-melt adhesives.Information provided by Zeon Chemicals L.P.
Molecular Weight 1.10e+6 g/mol
1.10e+6 g/mol
Zeon Chemicals Quintone® R100 Aliphatic Hydrocarbon Resin
C5 type (piperylene precursor). Gives well-balanced performance to adhesives; also suitable for hot melt adhesives.Information provided by Zeon Chemicals L.P.