Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 77 m²/g | 77 m²/g | Statistical thickness surface area; ASTM D 6556 |
Orion Engineered Carbons CORAX® N 326 ASTM Carbon Black Standard grade of furnace black in accordance with the requirements of ASTM D 1765Hard Black - tread grade, reinforcing carbon blackInformation provided by Orion Engineered Carbons. |
|||
Specific Surface Area | 77 m²/g | 77 m²/g | |
BASF Paliogen® Pink L 4790 Color Additive Description: Red pigment with very good weather fastnessSuitable for: Baking systems, Waterborn systems, Acrylic-isocyanate systems, and Airdrying systems.Information provided by BASF |