Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 75 m²/g | 75 m²/g | BET |
Nabaltec NABALOX® NO 201P Soft Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Specific Surface Area | 75 m²/g | 75 m²/g | Statistical thickness surface area; ASTM D 6556 |
Orion Engineered Carbons CK3 Carbon Black Produced by Degussa Gas Black ProcessInformation provided by Orion Engineered Carbons. |
|||
Specific Surface Area | 75 m²/g | 75 m²/g | |
Zircar Zirconia ZYBF-1 Zirconia Bulk Fiber Insulation Zirconia Bulk Fibers Type ZYBF are yttria stabilized zirconia fibers available in five different forms, all having useful properties up to 2200°C. These polycrystalline fibers can be vacuum formed .. |
|||
Specific Surface Area | 75 m²/g | 75 m²/g | |
Zircar Zirconia ZYBF-1 Zirconia Bulk Fiber Insulation Zirconia Bulk Fibers Type ZYBF are yttria stabilized zirconia fibers available in five different forms, all having useful properties up to 2200°C. These polycrystalline fibers can be vacuum formed .. |