Polymer Property : Specific Surface Area = 72 m²/g Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Surface Area 72 m²/g
72 m²/g
BASF Heligoen® Blue L 6920 Color Additive
Chemical Structure: Cu-phthalocyanine, Alpha StablePhysical form: PowderApplication: Pigment for PaintsInformation provided by BASF
Specific Surface Area 72 m²/g
72 m²/g
BASF Heligoen® Blue L 6900 Color Additive
Description: Standard-a-phthalocyanine blues for economic formulations (L 6920 is somewhat stronger than L 6900).Chemical Structure: Cu-phthalocyanine, alpha-stabPhysical form: PowderSuitable for: B..
Specific Surface Area 72 m²/g
72 m²/g
BASF Heligoen® Blue L 7460 Color Additive
Description: Metal free a-phthalocyanine blue especially for effect shadesChemical Structure: Cu-phthalocyanine, alpha-stab Physical form: PowderSuitable for: Baking systems, Waterborn systems, Acry..