Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Surface Area = 70 m²/g Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Surface Area 50 - 70 m²/g
50 - 70 m²/g
BET
Nabaltec NABALOX® NO 201 Calcined Aluminum Oxide
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
Specific Surface Area 60 - 70 m²/g
60 - 70 m²/g
NanoAmor 95%, OD/L: 40-60 nm/1-2 um Multi-Walled Carbon Nanotubes
Specific Surface Area 60 - 70 m²/g
60 - 70 m²/g
NanoAmor 99%, OD/L: 40-60 nm/1-2 um Multi-Walled Carbon Nanotubes
ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh..
Specific Surface Area 2.0 - 70 m²/g
2.0 - 70 m²/g
Terio Corporation TZC-15~80 CeO2-ZrO2
Information provided by TERIO Corporation.
Specific Surface Area 30 - 70 m²/g
30 - 70 m²/g
American Elements Aluminum Nanoparticles
General DescriptionAluminum (Al) Nanoparticles, nanodots or Nanopowder are black spherical high surface area metal particles. Nanoscale Aluminum Particles are typically 10-30 nanometers (nm) with sp..
Specific Surface Area 30 - 70 m²/g
30 - 70 m²/g
American Elements Beryllium Nanoparticles
General DescriptionBeryllium (Be) Nanoparticles, nanodots or nanopowder are spherical black high surface area particles. Nanoscale Beryllium Particles are typically 20-60 nanometers (nm) with specif..
Specific Surface Area 30 - 70 m²/g
30 - 70 m²/g
American Elements Magnesium Nanoparticles
General DescriptionMagnesium (Mg) Nanoparticles, nanodots or nanopowder are spherical black high surface area particles. Nanoscale Magnesium Particles are typically 20-60 nanometers (nm) with specif..
Specific Surface Area 30 - 70 m²/g
30 - 70 m²/g
American Elements Silicon Nanoparticles
General DescriptionSilicon (Si) Nanoparticles, nanodots or Nanopowder are spherical high surface area metal particles. Nanoscale Silicon Particles are typically 5-25 nanometers (nm) with specific su..
Specific Surface Area 30 - 70 m²/g
30 - 70 m²/g
American Elements Cobalt Nanoparticles
General DescriptionCobalt (Co) Nanoparticles, nanodots or nanopowder are spherical black high surface area particles. Nanoscale Cobalt Particles are typically 20-60 nanometers (nm) with specific sur..
Specific Surface Area 30 - 70 m²/g
30 - 70 m²/g
American Elements Copper Nanoparticles
General DescriptionCopper (Cu) Nanoparticles, nanodots or Nanopowder are black brown spherical high surface area metal particles. Nanoscale Copper Particles are typically 10-30 nanometers (nm) with ..
Copyright © lookpolymers.com All Rights Reserved