Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | >= 7.5 m²/g | >= 7.5 m²/g | Internal Method |
Solvay Specialty Polymers Algoflon® L203 Polytetrafluoroethylene (PTFE)
(Unverified Data**) Algoflon® L203 is a white PTFE micropowder comprising loose agglomerates of sub-micron sized particles. It is recommended for use as an additive in high quality oils and greases to reduce coefficie.. |
|||
Specific Surface Area | >= 7.5 m²/g | >= 7.5 m²/g | Internal Method |
Solvay Specialty Polymers Algoflon® L206 Polytetrafluoroethylene (PTFE)
(Unverified Data**) Algoflon® L206 is a white PTFE micropowder comprising loose agglomerates of sub-micron sized particles. It is specially recommended for use as an additive in elastomers (e.g. perfluoroelastomers) t.. |