Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 61 m²/g | 61 m²/g | |
BASF Heligoen® Green K 8683 Color Additive Chemical Structure: Cu-phthalocyanine chlorinate Application: Colourant for plastics; PVC-p, PVC-u, PUR, LD-PE, HD-PE, PP, PS, SB, SAN, PMMA, CA/CAB, and UPRecommendations for food applications: BgV.. |
|||
Specific Surface Area | 61 m²/g | 61 m²/g | |
BASF Heligoen® Green K 8730 Color Additive Chemical Structure: Cu-phthalocyanine chlorinate Application: Colourant for plastics; PVC-p, PVC-u, PUR, LD-PE, HD-PE, PP, PS, SB, SAN, PMMA, CA/CAB, and UPRecommendations for food applications: BgV.. |
|||
Specific Surface Area | 61 m²/g | 61 m²/g | |
BASF Heligoen® Green L 8730 Color Additive Description: Brilliant phthalocyanine greens, somewhat yellower than L 8690(L 8731 is especially for powder coatings)Chemical Structure: Cu-phthalocyanine, chlorinatePhysical form: PowderSuitable fo.. |
|||
Specific Surface Area | 61 m²/g | 61 m²/g | |
BASF Heligoen® Green L 8605 Color Additive Description: Bluish phthalocyanine greenChemical Structure: Cu-phthalocyanine, chlorinatePhysical form: PowderSuitable for: Baking systems, Waterborn systems, Acrylic-isocyanate systems, Acid curing.. |
|||
Specific Surface Area | 61 m²/g | 61 m²/g | |
BASF Heligoen® Green L 8731 Color Additive Description: Brilliant phthalocyanine greens, somewhat yellower than L 8690(L 8731 is especially for powder coatings)Chemical Structure: Cu-phthalocyanine, chlorinatePhysical form: PowderSuitable fo.. |