Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 58 m²/g | 58 m²/g | |
BASF Heligoen® Blue K 6902 Color Additive Chemical Structure: Cu-phthalocyanine alpha stab.Application: Colourant for plastics; PVC-p, PVC-u, PUR, LD-PE, HD-PE, PP, PS, SB, SAN, PMMA, PA, PETP, CA/CAB, and UPRecommendations for food applica.. |