Polymer Property : Specific Surface Area = 550 m²/g Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Surface Area >= 550 m²/g
>= 550 m²/g
BET
NanoScale NanoActive® Aluminum Oxide Plus
NanoActive Al2O3 Plus is produced using proprietary processes to obtain high specific surface area, high porosity (75% are mesopores), low density, weakly aggregated material possessing high adsorpt..