Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 37 m²/g | 37 m²/g | |
BASF Sico® Fast Red L 3855 Color Additive Description: Naphthol-AS-red pigment with good fastness properties in full shadeChemical Structure: Naphthol-AS-redSuitable for: Waterborn systems, Acrylic-isocyanate systems, Acid curing system, Am.. |