Physical Properties Metric English Comments
Specific Surface Area 100 - 360 m²/g
100 - 360 m²/g
Reade Advanced Materials Bentonite Powder (BaTiSi3O9)
Description: A rock composed essentially of a crystalline clay-like mineral formed by devitrification and the accompanying chemical alteration of a glassy igneous material, usually a tuff or volcani..