Polymer Property : Specific Surface Area = 36 m²/g Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Surface Area 36 m²/g
36 m²/g
BASF Heligoen® Blue L 6975 F Color Additive
Description: Brilliant a-phthalocyanine blue with high color strength and excellent rheology in systems containing aromatic solventsChemical Structure: Cu-phthalocyanine, alpha-stabPhysical form: Po..