Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | >= 230 m²/g | >= 230 m²/g | BET |
NanoScale NanoActive® Magnesium Oxide NanoActive MgO is produced using proprietary processes to obtain high specific surface area, small crystallite size material possessing high chemical reactivity, particularly at elevated temperature.. |
|||
Specific Surface Area | 230 m²/g | 230 m²/g | |
NanoAmor 95%, OD/ID/L: 8-15/3-5 nm/0.5-2 um Short Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Specific Surface Area | 230 m²/g | 230 m²/g | |
NanoAmor 95%, OD/ID: 8-15/3-5 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Specific Surface Area | 230 m²/g | 230 m²/g | |
NanoAmor 95%, OD: 8-15 nm COOH Functionalized Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Specific Surface Area | 230 m²/g | 230 m²/g | |
NanoAmor 95%, OD: 8-15 nm OH Functionalized Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |