Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 22.4 m²/g | 22.4 m²/g | |
Old Hickory 54-S Kentucky Ball Clay This ball clay is a multi- purpose clay that has excellent pressing, extrusion, and casting qualities. It has a moderately fine particle size distribution and the high plasticity and dry strength is.. |