Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Surface Area 21.4 m²/g
21.4 m²/g
Old Hickory MCB-11 Tennessee Ball Clay
A clay with excellent kaolin content and virtually no carbon content. It is highly plastic with excellent fired brightness and is an excellent clay for a variety of ceramic glaze and porcelain compo..