Polymer Property : Specific Surface Area = 2.58 m²/g Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Surface Area 2.58 m²/g
2.58 m²/g
Solvay Specialty Polymers Polymist® F-5A EX PTFE Powder Lubricant  (Unverified Data**)
Polymist® powders are a family of white free-flowing polytetrafluoroethylene powders for use as additives in other materials to enhance processing or end-use performance characteristics. Polymist ..