Polymer Property : Specific Surface Area = 2.2 m²/g
Polymer Property :
Specific Surface Area =
2.2 m²/g
Product List
Physical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties
Metric
English
Comments
Specific Surface Area
0.90
-
2.2
m²/g
0.90
-
2.2
m²/g
BET
Magyar Aluminum ALO-ExGB1 Alumina