Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 2.2 m²/g | 2.2 m²/g | BET |
Nyco ASPECT® 3000 Wollastonite High aspect ratio grade. It is available untreated or with a surface modification treatment.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. .. |