Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 19.3 m²/g | 19.3 m²/g | |
Old Hickory Dunn Tennessee Ball Clay Dunn clay is a selection originating from our Gleason, TN processing facility and is characterized by moderately high levels of kaolin interspersed with the presence of some carbon content. It is an.. |