Polymer Property : Specific Surface Area = 18.9 m²/g Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Surface Area 18.9 m²/g
18.9 m²/g
Old Hickory No. 5 Kentucky Ball Clay
No. 5 clay is a kaolinitic ball clay containing low levels of carbon. It provides high suspension and plasticity to a variety of ceramic formulations and is an excellent source of Al2O3 content. No...