Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 16 - 18 m²/g | 16 - 18 m²/g | BET |
H.C. Starck Grade BF 17 Silicon Carbide, SiC Beta SiC for sintering.Sliding bearingsSeal ringsWear partsKiln furniture, crucibles, heating elements, burner nozzles, heat exchangersSemiconductor handling partsComponents for wafer processing (su.. |