Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 17.0 m²/g | 17.0 m²/g | BET |
KaMin KaMin® 80B Kaolin Clay - Waterwashed KaMin® 80B is an economical, general purpose water-washed kaolin, with intermediate brightness. It is suitable for use in water-borne, solvent-borne and solvent-free paint, ink, and adhesive appl.. |
|||
Specific Surface Area | 17.0 m²/g | 17.0 m²/g | BET |
KaMin KaMin® 90 Kaolin clay - Waterwashed KaMin® 90 is a high brightness, fine particle size, general-purpose filler with moderate water demand. KaMin® 90 is ideally suited for solvent and water-borne paint, ink and adhesive applicati.. |
|||
Specific Surface Area | 17.0 m²/g | 17.0 m²/g | BET |
KaMin KaMin® 90B Kaolin Clay - Waterwashed KaMin® 90B is a high brightness, fine particle size, general-purpose filler with moderate water demand. KaMin® 90B is ideally suited for water-borne applications where high gloss, holdout and .. |
|||
Specific Surface Area | 17.0 m²/g | 17.0 m²/g | BET |
KaMin Polyfil® XB Kaolin Clay - Waterwashed Cost effective, kaolin extender offering improved consistency vs air floated clays, spray-dried bead form.Industry: Rubber & PlasticUses: Non-Black Rubber, General Rubber Goods, EPDM, Wire & CableIn.. |
|||
Specific Surface Area | 17.0 m²/g | 17.0 m²/g | BET |
KaMin Polyfil® F Kaolin Clay - Waterwashed Water washed kaolin clays such as Polyfil® F offer acid resistance, reinforcement, neutral pH, and extremely low crystalline silica and salt content. Polyfil® F is a moderate brightness water .. |
|||
Specific Surface Area | 17.0 m²/g | 17.0 m²/g | BET |
KaMin Polyfil® FB Kaolin Clay - Waterwashed Water washed kaolin clays such as Polyfil® FB offer acid resistance, reinforcement, neutral pH, and extremely low crystalline silica and salt content. Polyfil® FB is a moderate brightness wate.. |