Polymer Property : Specific Surface Area = 16 m²/g Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Surface Area 10 - 16 m²/g
10 - 16 m²/g
NYC YT3W Y2O3 Powder
Specific Surface Area 10 - 16 m²/g
10 - 16 m²/g
NYC YT3WP Y2O3 Granules
Specific Surface Area 6.0 - 16 m²/g
6.0 - 16 m²/g
BET
Magyar Aluminum ALO-BN-2F Alumina
Reactive Alumina
Specific Surface Area 6.0 - 16 m²/g
6.0 - 16 m²/g
BET
Magyar Aluminum ALO-BN-2S Alumina
Reactive Alumina
Specific Surface Area 10 - 16 m²/g
10 - 16 m²/g
BET
H.C. Starck Grade C Yttrium Oxide
Sintering additive for Si3N4 and ALNStabilizer for zirconias (PSZ) and insulating coatings (TBC`s)Catalyst carrierYttria stabilized zirconias electrolytes for solid oxide fuel cellsLuminescent mater..
Specific Surface Area 14 - 16 m²/g
14 - 16 m²/g
BET
H.C. Starck Grade UF 15 Silicon Carbide, SiC
Alpha SiC for sintering.Sliding bearingsSeal ringsWear partsKiln furniture, crucibles, heating elements, burner nozzles, heat exchangersSemiconductor handling partsComponents for wafer processing (s..