Polymer Property : Specific Surface Area = 13.5 m²/g
Polymer Property :
Specific Surface Area =
13.5 m²/g
Product List
Physical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties
Metric
English
Comments
Specific Surface Area
13.5
m²/g
13.5
m²/g
Imerys Allenâ„¢ G Kaolin
Allen G is an intermediate-grained kaolin used as a suspension aid in ceramic glazes.Information provided by Imerys