Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 9.0 - 11 m²/g | 9.0 - 11 m²/g | BET |
H.C. Starck Grade UF 10 Silicon Carbide, SiC Alpha SiC for sintering and hot-pressing.Sliding bearingsSeal ringsWear partsKiln furniture, crucibles, heating elements, burner nozzles, heat exchangersSemiconductor handling partsComponents for wa.. |
|||
Specific Surface Area | 7.0 - 11 m²/g | 7.0 - 11 m²/g | |
DuPont™ Kevlar® Aramid Pulp Sold as highly fibrillated, short (0.5-1mm) fibers. Kevlar® pulps are chopped fibers that can be used as specialty additives to enhance performance by providing excellent reinforcement and viscos.. |