Polymer Property : Specific Surface Area = 100 m²/g Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Surface Area 3.0 - 100 m²/g
3.0 - 100 m²/g
Terio Corporation TCZA-20~80 CeO2-Al2O3-ZrO2
Information provided by TERIO Corporation.