Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 1.6 m²/g | 1.6 m²/g | BET |
Nyco M400 WOLLASTOCOAT® Wollastonite Chemically treated grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
Specific Surface Area | 1.6 m²/g | 1.6 m²/g | BET |
Nyco MD400 WOLLASTOCOAT® Wollastonite Chemically treated grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
Specific Surface Area | 1.6 m²/g | 1.6 m²/g | BET |
Nyco NYAD® M400 Wollastonite Powdered grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance m.. |
|||
Specific Surface Area | 1.6 m²/g | 1.6 m²/g | BET |
Nyco NYAD® MD400 Wollastonite Powdered grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance m.. |