Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 1.2 m²/g | 1.2 m²/g | BET |
Nabaltec APYRAL® 20X Al(OH)3 APYRAL ® from Nabaltec is an environmentally friendly halogen free product which is used as a flame retardant filler in a wide variety of rubber and polymeric materials. During thermal decompositio.. |
|||
Specific Surface Area | 1.2 - 1.8 m²/g | 1.2 - 1.8 m²/g | BET |
Nabaltec NABALOX® NO 615-10 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Specific Surface Area | 1.2 - 1.8 m²/g | 1.2 - 1.8 m²/g | BET |
Nabaltec NABALOX® NO 625-10 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Specific Surface Area | <= 1.2 m²/g | <= 1.2 m²/g | BET |
Magyar Aluminum ALO-EL-4F Alumina Ground Alumina |
|||
Specific Surface Area | <= 1.2 m²/g | <= 1.2 m²/g | BET |
Magyar Aluminum ALO-EL-4S Alumina Ground Alumina |
|||
Specific Surface Area | <= 1.2 m²/g | <= 1.2 m²/g | BET |
Magyar Aluminum ALO-EL-7P Alumina Ground Alumina |
|||
Specific Surface Area | <= 1.2 m²/g | <= 1.2 m²/g | BET |
Magyar Aluminum ALO-P54-04 Alumina Alumina for Polishing |
|||
Specific Surface Area | 1.2 m²/g | 1.2 m²/g | |
Imerys G-200 HP Feldspar G-200 HP Feldspar is a high potassium aluminum silicate ground to 200 mesh for ceramic applications. G-200 HP offers high potassium content and low iron oxide per unit of alumina.Information provide.. |
|||
Specific Surface Area | 1.2 m²/g | 1.2 m²/g | Size C |
Vesta Ceramics SicoMill® Grade 2 Silicon Powder General Description:SicoMill® is a fine-grained silicon powder, specially developed for the ceramic industry. We have five standard grinding grades, but we can produce powders adapted to single cu.. |
|||
Specific Surface Area | 1.2 m²/g | 1.2 m²/g | Size C |
Vesta Ceramics SicoMill® Grade 4 Silicon Powder General Description:SicoMill® is a fine-grained silicon powder, specially developed for the ceramic industry. We have five standard grinding grades, but we can produce powders adapted to single cu.. |