Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 1.1 m²/g | 1.1 m²/g | BET |
Nyco ASPECT® 4000 Wollastonite ASPECT 4000 is available untreated or with a surface modification treatment.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive .. |
|||
Specific Surface Area | 1.1 m²/g | 1.1 m²/g | BET |
Nyco M200 WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Specific Surface Area | 1.1 m²/g | 1.1 m²/g | BET |
Nyco NYAD® M200 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Specific Surface Area | 1.1 m²/g | 1.1 m²/g | BET |
Nyco NYAD® MD200 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |