Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 0.50 - 1.0 m²/g | 0.50 - 1.0 m²/g | BET |
Nabaltec NABALOX® NO 105 Calcined Aluminum Oxide NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Specific Surface Area | 0.50 - 1.0 m²/g | 0.50 - 1.0 m²/g | BET |
Nabaltec NABALOX® NO 105 RA Calcined Aluminum Oxide NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Specific Surface Area | 0.10 - 1.0 m²/g | 0.10 - 1.0 m²/g | |
Momentive Performance Materials PolarTherm® PT110 Boron Nitride (BN) Powder Fine Hexagonal BN PowderWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic comp.. |