Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 0.25 m²/g | 0.25 m²/g | |
Momentive Performance Materials HCT-30 Titanium Diboride (TiB2) Powder A high purity powder, grade HCT has virtually no second phase contaminants and only low, controlled levels of carbon, oxygen and nitrogen. Alkalis, alkaline earth, and most metals are typically u.. |
|||
Specific Surface Area | 0.25 m²/g | 0.25 m²/g | |
Momentive Performance Materials HCT-30D Titanium Diboride (TiB2) Powder Grade HCT-30D is tailored for fabrication by the hot-pressing process. Its composition provides for ease and optimizes the mechanical properties of the component shapes.Titanium Diboride Powder .. |
|||
Specific Surface Area | 0.25 m²/g | 0.25 m²/g | |
Momentive Performance Materials HCT-40 Titanium Diboride (TiB2) Powder A high purity powder, grade HCT has virtually no second phase contaminants and only low, controlled levels of carbon, oxygen and nitrogen. Alkalis, alkaline earth, and most metals are typically u.. |