Physical Properties Metric English Comments
Particle Size 95 - 125 µm
95 - 125 µm
Lucite International Colacryl ® P2608 Specialty Polystyrene Resin
Cross-linked polystyrene resins have much higher thermal stability than conventional thermoplastic acrylic resin. Colacryl® P2608 is stable up to around 300°C.Suggested Uses:-Glass interleavan..
Particle Size 95 - 100 µm
95 - 100 µm
RP-0886
Solvay AG-RHOâ„¢ DEP-775 Surfactant
Description: Anti-drift agent as adjuvants or to formulate into plant protection productsIdentification: DERIVATIZED NATURAL POLYMER CAS: 497-19-8 Water Solubility: Quick hydrationAvailable in: Asia..
Particle Size 95 - 100 µm
95 - 100 µm
150 Mesh; PS-1-2
Solvay JAGUAR® 413 Surfactant
Description: Nonyl phenol based non ionic surfactant (70 EO)Chemical Name: GALACTOMANNAN BLENDCAS: 39421-75-5; 7631-86-9 Available in: Asia Pacific, Europe, Latin America and North AmericaApplicatio..
Particle Size 95 µm
95 µm
90th%
3M A16/500 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Particle Size 95 µm
95 µm
Effective Top Size
3M S15 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Particle Size 95 µm
95 µm
Average D50; Laser Diffraction
ALM D80-ST Nylon 11 SLS Prototyping Polymer
Unfilled, color stabilized nylon 11 material that is also stabilized to prevent premature thermal degradation. Parts produced from PA D80-ST exhibit superior mechanical properties. Relatively inexp..
Particle Size 95 µm
95 µm
Average D50; Laser Diffraction
ALM FR 106 Nylon 11 SLS Prototyping Polymer