Particle Size 9.2 µm
9.2 µm
Median
CIMBAR BARIMITE™ NO. 22 Barites High Purity Barite (BaSO4)
Barimite Products are natural, off-white barites produced in Cartersville, Georgia. Cimbar's broad range of Barimite products are clean, high purity, high specific gravity, low solubility and chemi..