Polymer Property : Particle Size = 8.9 µm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Size 8.9 - 28 µm
8.9 - 28 µm
d50
Indium Corp. In(OH)3 Crystalline Indium Hydroxide
Indium Acetate is a white powder. Crystalline Form: Primary particles range from 1 to 5 microns in size. They are cubic in shape and form agglomerates up to approximately 35 microns.PropertiesChe..