Polymer Property : Particle Size = 8.0 µm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Size 4.0 - 8.0 µm
4.0 - 8.0 µm
d50
Magyar Aluminum ALO-P90-06 Alumina
Alumina for Polishing
Particle Size 4.0 - 8.0 µm
4.0 - 8.0 µm
d50
Magyar Aluminum ALO-P95-06 Alumina
Alumina for Polishing
Particle Size 2.7 - 8.0 µm
2.7 - 8.0 µm
d10
Indium Corp. Standard ITO Indium Tin Oxide
Indium Tin Oxide (ITO, or tin-doped indium oxide) is a mixture of indium(III) oxide and tin(IV) oxide, typically 90% indium oxide, 10% tin oxide by weight. In powder form it is yellow-green in colo..
Particle Size 4.0 - 8.0 µm
4.0 - 8.0 µm
D 50%; Laser Light Diffraction per ASTM C1070
H.C. Starck Type I Pure Molybdenum MIMP Powder
Description of Product: Highly deagglomerated high purity molybdenum powder for any applications requiring the most finely deagglomerated powders like paste or metal injection molding applications...
Particle Size 4.5 - 8.0 µm
4.5 - 8.0 µm
d90, Guaranteed
TIMCAL TIMREX® LSG6 Natural Graphite
TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-..