Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 68 - 77 µm | 68 - 77 µm | 50% |
H.C. Starck Amperit® 827.6 Zirconium Oxide-Yttrium Oxide 93-7 (ZrO2-Y2O3) |
|||
Particle Size | 68 - 77 µm | 68 - 77 µm | 50% |
H.C. Starck Amperit® 832.6 Zirconium Oxide-Yttrium Oxide 93-7 (ZrO2-Y2O3) |