Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 65 - 75 µm | 65 - 75 µm | 90% |
H.C. Starck Amperit® 519.088 Agglomerated, Sintered Tungsten Carbide-Cobalt 88-12 (WC-CO) |
|||
Particle Size | 65 - 75 µm | 65 - 75 µm | 90% |
H.C. Starck Amperit® 526.088 Agglomerated, Sintered Tungsten Carbide-Cobalt (WC-Co) 83-17 |
|||
Particle Size | 65 - 75 µm | 65 - 75 µm | 90% |
H.C. Starck Amperit® 527.088 Agglomerated, Sintered Tungsten Carbide-Cobalt (WC-Co) 83-17 |
|||
Particle Size | 65 - 75 µm | 65 - 75 µm | 90% |
H.C. Starck Amperit® 558.088 Tungsten Carbide-Cobalt-Chromium 86-10-4 (WC-Co-Cr) |
|||
Particle Size | 55 - 75 µm | 55 - 75 µm | |
Lucite International Colacryl ® D80 Acrylic Dental Resin A range of Methyl Methacrylate polymers designed for use as standard heat-curing denture base resins.Features: Fine free-flowing bead polymers containing residual peroxide initiator; Curing cycles f.. |
|||
Particle Size | 55 - 75 µm | 55 - 75 µm | |
Lucite International Colacryl ® TS 1672 Acrylic Orthodontic Polymer A range of methacrylate based copolymers designed for the manufacture of high quality orthodontic dental resins.Features: Excellent dry flow characteristics; Closely controlled particle size; Contai.. |
|||
Particle Size | 65 - 75 µm | 65 - 75 µm | 90% |
H.C. Starck Amperit® 588.088 Chromium Carbide-Nickel Chromium 75-25 (Cr3C2-NiCr) 53/20 µm |
|||
Particle Size | 65 - 75 µm | 65 - 75 µm | 90% |
H.C. Starck Amperit® 547.074 Tungsten Carbide-Nickel 88-12 (WC-Ni) |